Stoneware: Good basic for practice and production.
Product Details
Sibelco’s terracotta studio body.
Good for handbuilding and throwing
Firing temperature: 1000°C – 1280°C
Chamotte: none
Shrinkage wet to dry: 4,8%
Firing shrinkage:
@ 1140°C – 4,5%
@ 1200°C – 5%
@ 1280°C – 5%
Waterabsorption:
@ 1140°C – 4,2%
@ 1200°C – 3%
@ 1280°C – 1%